Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 444.7 MPa @Temperature 427 °C |
64500 psi @Temperature 801 °F |
Autogenously Welded plate, 1.6mm thick |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |