Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 68.3 MPa @Temperature 100 °C |
9910 psi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Tensile Strength at Break | 68.3 MPa @Temperature 100 °C |
9910 psi @Temperature 212 °F |
2; ISO 527-2 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |