Polymer Property : Tear Strength = 0.390 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam
Information provided by Rogers Corporation.
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® 4790-79SP-15012 Urethane Shock Pad Foam
Information provided by Rogers Corporation.
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® ThinStik Soft Seal 15-06021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® ThinStik Soft Seal 15-06030 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® ThinStik™ 92-09020 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to ABS; ASTM D1000
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..
Tear Strength 0.390 kN/m

@Time 259000 sec
2.23 pli

@Time 72.0 hour
Peel Adhesion, 180° Peel, to Acrylic; ASTM D1000
Rogers Corporation Poron® ThinStik™ 92-12020 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..