Polymer Property : Rupture Strength = 9000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Rupture Strength 62.1 MPa

@Temperature 927 °C,
Time 270000 sec
9000 psi

@Temperature 1700 °F,
Time 75.0 hour
Special Metals INCONEL® alloy N06230 Ni-Cr-W-Mo Alloy
INCONEL® alloy N06230 (UNS N06230 / W.Nr. 2.4733) is a carbide strengthened nickel-chromium-tungsten-molybdenum alloy with an exceptional combination of strength, stability, and resistance to cor..