Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1150 MPa | 167000 psi | ASTM D790A |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Flexural Modulus, 1% Secant | 1150 MPa | 167000 psi | ASTM-D790 |
Braskem GP5550 HDPE High Density Extrusion Polyethylene GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications .. |