Flexural Modulus, 1% Secant 1206 MPa
174900 psi
ASTM D790
Flint Hills P5G2K-096 Random Copolymer Polypropylene
Features: Excellent clarity. Product does not contain animal derived components. Phthalate-freeApplications: Thermoforming, extrusion blow molding, injection blow molding, stretch blow molding, ..