Polymer Property : Flexural Modulus, 1% Secant = 136000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 938 MPa
136000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP8244E1 Polypropylene Homopolymer
Product Description: A high crystallinity, high impact copolymer resin designed for injection molded applications requiring excellent processing attributes.Availability: North America Features:Bala..