Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1390 MPa | 201000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP5341E1 Polypropylene Homopolymer Product Description: A low melt flow rate that provides high melt strength and resistance to softening at elevated temperature.Availability: North America Features:Low FlowUses: Automotive Applic.. |