Polymer Property : Flexural Modulus, 1% Secant = 148000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1020 MPa
148000 psi
ASTM D790A
Dow 6D20 Polypropylene Random Copolymer Resin
OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr..
Flexural Modulus, 1% Secant 1020 MPa
148000 psi
ASTM D790A
Dow R131-02A Polypropylene Random Copolymer Resin
DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..
Flexural Modulus, 1% Secant 1020 MPa
148000 psi
ASTM D790A
Dow R132-02A Polypropylene Random Copolymer Resin
DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier..