Polymer Property : Flexural Modulus, 1% Secant = 1510 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1510 MPa
219000 psi
ASTM D790A
SABIC PP 578P Polypropylene Homopolymer for Injection Molding
Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr..