Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1530 MPa
222000 psi
ASTM D790A
SABIC PP 510P Polypropylene Homopolymer for Fiber Applications
Product Description: PP 510P is a homopolymer specially designed for fiber extrusion applications with the following features:Consistent processabilityGood thread line stabilityGood color consisten..
Flexural Modulus, 1% Secant 1530 MPa
222000 psi
0.5 in/min; ASTM D790B
ExxonMobil AXO3BE3 Polypropylene Homopolymer
Product Description: A high crystallinity, medium impact copolymer resin designed for injection-molded automotive interior applications and large appliance parts applications requiring high melt fl..
Flexural Modulus, 1% Secant 1530 MPa
222000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP1024E4 Homopolymer
Product Description: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection moldingAvailability: North America Features:Autoclave SterilizableEthylene Oxide Steriliz..