Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1740 MPa | 252000 psi | ASTM D790 |
Flint Hills P4G4K-205 Homopolymer Polypropylene Features: Clarified material. Product does not contain animal derived components. Phthalate-free.Applications: Cast FilmInformation provided by Flint Hills Resources. |
|||
Flexural Modulus, 1% Secant | 1740 MPa | 252000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP1024E4 Homopolymer Product Description: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection moldingAvailability: North America Features:Autoclave SterilizableEthylene Oxide Steriliz.. |
|||
Flexural Modulus, 1% Secant | 1740 MPa | 253000 psi | 0.05 in/min; ASTM D790A |
ExxonMobil PP1074KNE1 Polypropylene Homopolymer Product Description: A nucleated, medium flow rate homopolymer resin with mold release and anti-static properties. It is suitable for general purpose injection molding.Availability: North America .. |