Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 20.0 MPa
2900 psi
ASTM D790
ExxonMobil Escorene™ UL 7741 Ethylene Vinyl Acetate Copolymer
Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends..