Flexural Modulus, 1% Secant 200 MPa
29000 psi
ASTM-D790
Braskem G803 LDPE Injection Molding Polyethylene
G803 is a low-density polyethylene with excellent processability, high fluidity, and dimensional stability. It does not contain additives. Its applications include: lids, closures, and general purp..