Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 2070 MPa | 300000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP7815E1 Polypropylene Homopolymer Product Description: A high crystallinity, low impact strength copolymer resin designed for compounding base or injection molding applications requiring high melt flow rate.Availability: North Amer.. |
|||
Flexural Modulus, 1% Secant | 2070 MPa | 300000 psi | ASTM D790B |
Braskem INSPIRE™ 404 Performance Polypropylene Polymer INSPIRE 404 Performance Polymer is a propylene-based resin intended for use in thermoforming applications where exceptional stiffness, clarity and heat resistance is desired. The high stiffness of .. |