Polymer Property : Flexural Modulus, 1% Secant = 208000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1430 MPa
208000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP4712E1 Polymer Grade for Oriented Film
Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo..