Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 1470 MPa

@Temperature 23.0 °C
213000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Ineos H02G-02 Polypropylene Homopolymer
This is a homopolymer designed for extrusion and film. It exhibits good extrusion and film orientation behavior. This material meets the requirements of the U.S. Food and Drug Administration as sp..