Polymer Property : Flexural Modulus, 1% Secant = 38.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 38.6 MPa
5600 psi
ASTM D790
ExxonMobil Escorene™ UL 7521 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 7521 is a high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesiv..