Flexural Modulus, 1% Secant 490 MPa
71000 psi
ASTM D790
ExxonMobil LLDPE LL 6301RQ Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra..
Flexural Modulus, 1% Secant 490 MPa
71000 psi
ASTM D790
ExxonMobil LLDPE LL 6301XR Molding Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 6301 series are medium flow LLDPE grades, with a relatively molecular weight, resulting in molded articles which are very tough and exhibit excellent environmental stress cra..