Flexural Modulus, 1% Secant 359 MPa
52000 psi
ASTM D790
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin
Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a h..