Polymer Property : Flexural Modulus, 1% Secant = 59.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 59.3 MPa
8600 psi
ASTM D790
ExxonMobil Vistamaxx™ 3000 Propylene-based Elastomer
Product Description: Vistamaxx 3000 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Technology. It has moderate elastomeric properties, is easy to ..