Polymer Property : Flexural Modulus, 1% Secant = 700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 700 MPa
102000 psi
ASTM D790
Braskem PB 208 LDPE Injection Molding Polyethylene
Description: PB208 is a low density polyethylene with no additives. This grade shows excellent processability being indicated for low viscosity required applications. Injection molded products with ..
Flexural Modulus, 1% Secant 700 MPa
102000 psi
ASTM D790
Braskem PB208 Injection Molding Low Density Polyethylene
Injected lids and caps; Large flat surface injected pieces.Information provided by Braskem.