Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 51.7 MPa | 7500 psi | ASTM D790 |
ExxonMobil Escorene™ LD 723.28 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 723.28 is a 18.5 wt% vinyl acetate copolymer suitable for injection molding and compounding applications.Availability: Latin America, North America and South A.. |