Polymer Property : Flexural Modulus, 1% Secant = 972 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 972 MPa
141000 psi
0.05 in/min; ASTM D790A
ExxonMobil PP9122 Polypropylene Homopolymer
Product Description: A random copolymer resin designed for extrusion blow molding applications and thermoforming of medical and other specialty devices and packaging. It has excellent organoleptics..