K (wear) Factor 0.604 x 10-8 mm³/N-M
0.300 x 10-10 in³-min/ft-lb-hr
Lubricated: 4 m/s, 5.2 MPa (800 fpm, 750 psi); ASTM D3702
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest..