Polymer Property : K (wear) Factor = 0.806 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 0.806 x 10-8 mm³/N-M
0.400 x 10-10 in³-min/ft-lb-hr
Lubricated: 4 m/s, 5.2 MPa (800 fpm, 750 psi); ASTM D3702
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..