Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 205 x 10-8 mm³/N-M | 102 x 10-10 in³-min/ft-lb-hr | QTM 55010 |
Quadrant EPP Ketron® CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to ho.. |