Polymer Property : K (wear) Factor = 106 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 214 x 10-8 mm³/N-M
106 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Lubricomp® EL-4030 Polyetherimide, PTFE Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
K (wear) Factor 214 x 10-8 mm³/N-M
106 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing 15% PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 214 x 10-8 mm³/N-M
106 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Asia Pacific)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.
K (wear) Factor 214 x 10-8 mm³/N-M
106 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP EL003 PEI (Europe-Africa-Middle East)
LNP LUBRICOMP* EL003 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.