Polymer Property : K (wear) Factor = 130 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 262 x 10-8 mm³/N-M
130 x 10-10 in³-min/ft-lb-hr
40psi, 50ft/min; tested in accordance with LNP WI-0687
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
K (wear) Factor 262 x 10-8 mm³/N-M
130 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI
LNP THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing 30% Glass Fiber.