Polymer Property : K (wear) Factor = 142 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 10.0 - 142 x 10-8 mm³/N-M
4.96 - 70.6 x 10-10 in³-min/ft-lb-hr
Average value: 39.6 x 10<sup>-8</sup> mm³/N-M Grade Count:8
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum..