Polymer Property : K (wear) Factor = 15.9 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 32.0 x 10-8 mm³/N-M
15.9 x 10-10 in³-min/ft-lb-hr
at 5000 psi - fpm PV; ASTM D3702
3M Dyneon™ CC144/S PTFE, 40% Bronze Filled  (discontinued **)
Product Form: Brown, non-pelletized powder. Applications include bearings, rider rings, and piston rings.Data provided by Dyneon.