Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : K (wear) Factor = 153 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 308 x 10-8 mm³/N-M
153 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DP001E PC
LNP* LUBRICOMP* DP001E is a Polycarbonate base resin containing 5% PTFE/Silicone. Added features are: Internally Lubricated, Easy Molding.
Copyright © lookpolymers.com All Rights Reserved