Polymer Property : K (wear) Factor = 179 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 361 x 10-8 mm³/N-M
179 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY DF204 PC
LNP* LUBRILOY* DF204 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added feature of th is grade is: Wear Resistant.