Polymer Property : K (wear) Factor = 181 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 91.0 - 181 x 10-8 mm³/N-M
45.2 - 90.0 x 10-10 in³-min/ft-lb-hr
Average value: 134 x 10<sup>-8</sup> mm³/N-M Grade Count:3
Overview of materials for Nylon 6, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria..