Polymer Property : K (wear) Factor = 20.0 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 10.0 - 20.0 x 10-8 mm³/N-M
4.96 - 9.93 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide
PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon®
K (wear) Factor 16.0 - 20.0 x 10-8 mm³/N-M
7.94 - 9.93 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
K (wear) Factor 10.0 - 20.0 x 10-8 mm³/N-M
4.96 - 9.93 x 10-10 in³-min/ft-lb-hr
at PV 100; ASTM D3702
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber
PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re..