Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 8.06 - 500 x 10-8 mm³/N-M | 4.00 - 248 x 10-10 in³-min/ft-lb-hr | Average value: 203 x 10<sup>-8</sup> mm³/N-M Grade Count:12 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |