Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 60.0 x 10-8 mm³/N-M | 29.8 x 10-10 in³-min/ft-lb-hr | at PV 100; ASTM D3702 |
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss.. |