Polymer Property : K (wear) Factor = 34.0 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 68.5 x 10-8 mm³/N-M
34.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC
LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release.
K (wear) Factor 68.5 x 10-8 mm³/N-M
34.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific)
LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release.