Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 72.5 x 10-8 mm³/N-M | 36.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP REL22 PA 66 LNP* LUBRICOMP* REL22 is a compound based on Nylon 66 resin containing 10% Carbon Fiber, 10% PTFE. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
K (wear) Factor | 72.5 x 10-8 mm³/N-M | 36.0 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66 LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant |