Polymer Property : K (wear) Factor = 473 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 473 x 10-8 mm³/N-M
235 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.