Polymer Property : K (wear) Factor = 57.0 x 10-10 in³-min/ft-lb-hr Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 115 x 10-8 mm³/N-M
57.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant.
K (wear) Factor 115 x 10-8 mm³/N-M
57.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific)
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant.