Mechanical Properties Metric English Comments
K (wear) Factor 58.4 x 10-8 mm³/N-M
29.0 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubricomp OFG26XXP PPS - Linear
LNP* Lubricomp* OFG26XXP is a compound based on Linear PPS containing Glass Fiber and Graphite Powder. Characteristics of this grade are Internally Lubricated.This data was supplied by SABIC-IP for..
K (wear) Factor 58.4 x 10-8 mm³/N-M
29.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 58.4 x 10-8 mm³/N-M
29.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D 3702 Modified
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
K (wear) Factor 58.4 x 10-8 mm³/N-M
29.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
K (wear) Factor 58.4 x 10-8 mm³/N-M
29.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare