Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 751 x 10-8 mm³/N-M | 373 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP OF008 PPS - Linear LNP* THERMOCOMP* OF008 is a compound based on PPS - Linear resin containing 40% Glass Fiber. |
|||
K (wear) Factor | 751 x 10-8 mm³/N-M | 373 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
SABIC Innovative Plastics LNP THERMOCOMP OF008H PPS - Linear LNP* THERMOCOMP* OF008H is a compound based on PPS - Linear containing 40% Glass Fiber. Characteristics of this grade are: Healthcare. |
|||
K (wear) Factor | 751 x 10-8 mm³/N-M | 373 x 10-10 in³-min/ft-lb-hr | 40psi, 50ft/min; tested in accordance with LNP WI-0687 |
LNP Thermocomp® OF-1008 Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |