Polymer Property : K (wear) Factor = 9.30 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 9.30 x 10-8 mm³/N-M
4.62 x 10-10 in³-min/ft-lb-hr
LATI Latilub 62-10T PA6
Self-lubricating product based on Polyamide 6 (PA6). PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..