Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.185 MPa @Strain 30.0 % |
26.8 psi @Strain 30.0 % |
ASTM D413 |
Objet FullCure® 930 Tango Plus Resin for Rapid Prototyping Information provided by American Precision Prototyping, LLC |