Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 68.9 MPa @Thickness 1.57 mm |
10000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP315 Cotton Fabric Description: Canvas phenolic laminate with graphite added as a solid lubricant. This material has improved wear properties under certain conditions. Material is conductive to electricity and should .. |
|||
Tensile Strength, Yield | 68.9 MPa @Thickness 1.57 mm |
10000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP320 Cotton Fabric Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape.. |
|||
Tensile Strength, Yield | 68.9 MPa @Thickness 1.57 mm |
10000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP318 Cotton Fabric Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t.. |