Tensile Strength, Yield 108 MPa

@Strain 0.200 %,
Temperature 400 °C
15700 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 108 MPa

@Strain 0.200 %,
Temperature 400 °C
15700 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 108 MPa

@Strain 0.200 %,
Temperature 400 °C
15700 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 108 MPa

@Strain 0.200 %,
Temperature 300 °C
15700 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..
Tensile Strength, Yield 108 MPa

@Strain 1.00 %,
Temperature 600 °C
15700 psi

@Strain 1.00 %,
Temperature 1110 °F
EN min.; EN 10002-5
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..