Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 109.6 MPa @Temperature 871 °C |
15900 psi @Temperature 1600 °F |
Autogenously Welded plate, 1.6mm thick |
Special Metals INCOLOY® alloy 864 INCOLOY® alloy 8684 (UNS S35135) was specifically developed for automotive exhaust system flexible couplings, EGR tubes, manifolds and tailpipes. It exhibits excellent fatigue resistance, therma.. |