Mechanical Properties Metric English Comments
Tensile Strength, Yield 116 MPa

@Strain 1.00 %,
Temperature 400 °C
16800 psi

@Strain 1.00 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 116 MPa

@Strain 1.00 %,
Temperature 400 °C
16800 psi

@Strain 1.00 %,
Temperature 752 °F
EN min.; EN 10002-5
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 116 MPa

@Strain 0.200 %,
Temperature 200 °C
16800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 116 MPa

@Strain 0.200 %,
Temperature 200 °C
16800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 116 MPa

@Strain 0.200 %,
Temperature 200 °C
16800 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..