Polymer Property : Tensile Strength, Yield = 12.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.8 MPa

@Strain 500 %
1860 psi

@Strain 500 %
NBR Conductive Hose Compound
TIMCAL ENSACO™ 250G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Tensile Strength, Yield 12.8 MPa

@Strain 50.0 %
1860 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.8 MPa

@Strain 50.0 %
1860 psi

@Strain 50.0 %
ISO 527-1/-2
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Tensile Strength, Yield 12.8 MPa

@Strain 300 %
1860 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 685A15N Polyester Type Polyurethane Elastomer
This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes..